Aluminum Basics

What Is Aluminum Extrusion? The Process in 10 Steps

Aluminum extrusion pushes a heated, solid aluminum billet through a shaped steel die to make a long profile with the same cross-section along its length.

Product guides and technical content

Aluminum extrusion pushes a heated but solid aluminum billet through a shaped steel die with a hydraulic press, producing a long profile with a constant cross-section. The main steps are die design, billet and die heating, pressing, quenching, stretching, cutting, aging to temper, finishing and inspection. The press size limits how wide and heavy the profile can be.

Aluminum extrusion pushes a heated but still solid aluminum billet through a shaped steel die with a hydraulic press. The result is a long profile with the same cross-section along its whole length.

It works much like squeezing toothpaste from a tube: the shape of the opening becomes the shape of the product. The aluminum is never melted during extrusion; it is softened by heat so that it flows under pressure.

Extrusion can produce simple bars and tubes as well as complex profiles with channels, ribs and hollow chambers. That is why it is used for windows, facades, machine frames, solar mounting systems, vehicles and furniture. Below is the process in ten steps, followed by profile types and design limits. For Bor's own presses, see our aluminum extrusion page.

The Aluminum Extrusion Process in 10 Steps

Step 1: Profile design

Everything starts with the cross-section drawing. The designer sets the shape, wall thicknesses, tolerances, alloy and temper. Good extrusion design keeps wall thicknesses as even as possible and avoids very deep, narrow channels, which are hard to fill.

Step 2: Die making

A die is machined from hardened tool steel, usually by CNC machining and wire cutting. Solid profiles use flat dies; hollow profiles use dies with a mandrel, in which the metal splits and welds together again inside the die.

Step 3: Billet preparation and heating

A billet, a round log of aluminum alloy cut to length, is heated in a furnace. For common 6xxx alloys the billet is typically heated to around 450–500 °C, hot enough to flow under pressure but well below the melting point. The billet's chemistry and homogenization strongly affect the result; see billet casting and what to specify.

Step 4: Die and container preheating

The die and the press container are also preheated, so the aluminum does not cool and stick when it touches them.

Step 5: Pressing

The billet is loaded into the container, and the press ram pushes it through the die. The profile leaves the die as a continuous length. In direct extrusion the billet moves through the container; in indirect extrusion the die moves into the billet, which reduces friction.

Step 6: Quenching

As the profile runs out onto the table, it is cooled by air or water. The cooling rate is part of the heat treatment and affects the final strength.

Step 7: Stretching

Each length is gripped at both ends and stretched slightly. This straightens the profile and relieves internal stress.

Step 8: Cutting

Profiles are sawn to the ordered length. At Bor, extruded profiles can be up to 12 m long.

Step 9: Aging

Heat-treatable 6xxx alloys are aged in an oven to reach their final temper, for example T5 or T6. Aging precipitates fine particles in the metal and raises its strength.

Step 10: Finishing, machining and inspection

Profiles can then be anodized, powder coated or machined. Dimensions and properties are checked against the drawing and standards such as EN 755 and EN 12020 in Europe or ASTM B221 and ANSI H35.2 in the United States.

Types of Extruded Profiles

TypeDescriptionExamples
SolidNo enclosed voidsBars, angles, T-sections, flat trims
Semi-hollowA partly enclosed void with a narrow gapSome channels and grooves
HollowOne or more fully enclosed voidsTubes, window frame chambers, multi-chamber profiles

What Limits the Size of a Profile?

The press does. Press size is often given in inches, which refers to the diameter of the billet it takes. A larger press uses a larger billet and can make wider, heavier profiles. Each press has a maximum circumscribing size that a profile must fit within.

Bor pressForceLargest cross-section envelopes (mm)
5-inch (×2)1,100 tons151 × 14 · 117 × 55 · 90 × 90
7-inch1,880 tons220 × 20 · 170 × 80 · 130 × 130
9-inch2,800 tons340 × 40 · 260 × 80 · 180 × 180

The exact limit depends on the profile shape and wall thickness. The full table is on our extrusion page.

Is Extruded Aluminum Strong?

Extruded aluminum can be strong enough for structural use, but it is not stronger than steel. Strength depends on the alloy and temper: 6063-T5 is moderate in strength and gives an excellent surface, while 6061-T6 and 6082-T6 are used where higher strength is needed. Extrusion lets designers put material exactly where it is needed, so a well-designed profile can be both light and stiff. See steel vs. aluminum for a full comparison.

Advantages of Aluminum Extrusion

  • Complex cross-sections in one piece, with channels, screw ports and snap fits built in.
  • Relatively low die cost compared with many other metal forming tools.
  • Long lengths with a consistent cross-section.
  • Good surface quality, suitable for anodizing and coating.
  • Profiles can be fully recycled.

Extrusion is different from casting, where molten aluminum is poured into a mold. Our article aluminum extrusion vs. casting explains the difference.

Extrusion at Bor Alüminyum

Bor Alüminyum extrudes profiles from its own billets on four presses: two 5-inch, one 7-inch and one 9-inch. Annual capacity is 45,000 metric tons, and more than 7,000 profile types have been produced. Standard profiles can be ordered by catalog code; custom profiles are made to your drawing. Browse the aluminum profile range or read about custom aluminum extrusion.

Frequently Asked Questions

Is aluminum melted during extrusion?

No. The billet is heated to make it soft enough to flow, but it stays solid while it is pushed through the die.

What alloys are used for extrusion?

Mostly 6xxx-series alloys such as 6060, 6063, 6061 and 6082, because they extrude well and gain strength through heat treatment.

What do T5 and T6 mean?

They are tempers. T5 means cooled from extrusion and artificially aged; T6 means solution heat treated and artificially aged, which usually gives higher strength.

How long can extruded profiles be?

That depends on the plant. At Bor, profiles can be extruded up to 12 m long and cut to the length you order.

Bor USA Content Team

Author: Bor USA Content Team

The Bor USA Content Team writes and maintains the guides on this site. Articles draw on the production experience of Bor Alüminyum, the family-owned aluminum extrusion manufacturer founded in 1997 in Çerkezköy, Türkiye, and on BorUSA Aluminum LLC's work with customers in the United States from Fort Lauderdale, Florida. Technical statements refer to published standards such as EN 755 and EN 12020.

0 comments

Leave a comment

Your comment will be published after review.

Your rating:

Bor USA

Get a Quote

Tell us briefly what you need and we will get back to you with a quote.

Your details are only used to respond to this request. Privacy Notice